Cruisers Forum
 

Go Back   Cruisers & Sailing Forums > Engineering & Systems > Electrical: Batteries, Generators & Solar
Cruiser Wiki Click Here to Login
Register Vendors FAQ Community Calendar Today's Posts Log in

Reply
  This discussion is proudly sponsored by:
Please support our sponsors and let them know you heard about their products on Cruisers Forums. Advertise Here
 
Thread Tools Search this Thread Rate Thread Display Modes
Old 27-12-2018, 08:35   #16
Commercial Member
 
CharlieJ's Avatar

Cruisers Forum Supporter

Join Date: Dec 2008
Location: St. Petersburg, FL
Boat: Gulfstar Long Range Trawler; 53'; BearBoat
Posts: 1,535
Re: Stray- Current Corrosion, or Galvanic Corrosion, or?????...Help

The damage exhibited by the photos does not appear to be caused by stray current, also known as electrolytic corrosion and is generally caused by the victim vessel.
Stray current corrosion is generally a DC phenomenon, it is very destructive to the affected underwater component and generally very fast in its manifestation: days and weeks.
Galvanic corrosion is a slow, low voltage process that takes months and years to manifest itself. An everyday example is the shaft anode on a propulsion shaft.

A high quality bonding system includes:
>> Electrical connection to each u/w component
>> Using AWG 8 stranded wire
>> With each connection <1 Ω resistance
>> Final connection to the hull (plate) anode

One of the benefits of a high quality bonding system is that it all but eliminates the possibility of stray current corrosion of the underwater metal components. With the u/w components all bonded together, they are all at the same electrical potential so current cannot flow. Touch a B+ to a well bonded boat's u/w component and...no corrosion will occur.

Continuity Testing: Most DMMs that mesure continuity will indicate continuity when the resistance is < 100 to 200 Ω. That just isn't good enough in corrosion mitigation. While the boat is out of the water, make up some long test leads and check for resistance between your u/w components. All should be <1Ω; correct all that are not.

With the exception of the strut, it appears that you have a paint system failure, as BoatPoker postulates. Insulate the metal components from the copper based paint by applying Interlux 2000/3000 to a properly prepared u/w component and I believe your problem will resolve.

The strut appears to be under-protected by the plate anode and can be corrected by correctly bonding it as discussed above.

BTW, "electrolysis" is the dissociation of water into its constituent parts and has nothing to do with marine corrosion.

For what its worth, I am an ABYC Corrosion Technician and a former ABYC Certification Instructor.

PM me if you have any questions.
__________________
Charlie Johnson
ABYC Master Technician
JTB Marine Corporation
"The Devil is in the details and so is salvation."
CharlieJ is offline   Reply With Quote
Old 27-12-2018, 11:05   #17
Registered User

Join Date: Oct 2012
Location: Gulf Harbour, New Zealand
Boat: Farr Phase 4, 12.8m
Posts: 1,160
Re: Stray- Current Corrosion, or Galvanic Corrosion, or?????...Help

Have you changed your anode size, type or location lately? This looks like paint blasting due to over protection? The half cell test will tell you....
__________________
Matt Paulin
Neptune's Gear is offline   Reply With Quote
Old 27-12-2018, 12:04   #18
Registered User

Join Date: May 2009
Location: Massachusetts
Boat: 40' Silverton Aftcabin with twin Crusaders
Posts: 1,791
Re: Stray- Current Corrosion, or Galvanic Corrosion, or?????...Help

Quote:
Originally Posted by Neptune's Gear View Post
Have you changed your anode size, type or location lately? This looks like paint blasting due to over protection? The half cell test will tell you....


Would you explain how a half cell will tell if over protected
foggysail is offline   Reply With Quote
Old 27-12-2018, 12:16   #19
Commercial Member
 
CharlieJ's Avatar

Cruisers Forum Supporter

Join Date: Dec 2008
Location: St. Petersburg, FL
Boat: Gulfstar Long Range Trawler; 53'; BearBoat
Posts: 1,535
Re: Stray- Current Corrosion, or Galvanic Corrosion, or?????...Help

Over protection requires an excellent bonding system connected to the hull anode
__________________
Charlie Johnson
ABYC Master Technician
JTB Marine Corporation
"The Devil is in the details and so is salvation."
CharlieJ is offline   Reply With Quote
Old 27-12-2018, 12:59   #20
Registered User
 
Wood's Avatar

Join Date: Feb 2016
Location: Portsmouth, NH
Boat: Bayliner, 4588, 45'
Posts: 207
Re: Stray- Current Corrosion, or Galvanic Corrosion, or?????...Help

Quote:
Originally Posted by foggysail View Post
Would you explain how a half cell will tell if over protected

Assuming aluminum anodes on fiberglass hull 1/2 cell should read -1050 mv or so. Over protection would show > -1200mv or thereabouts.



You can check specs for steel hulls / or different anodes on places like boatzincs.com
__________________
Irony
4588 Bayliner
Portsmouth, NH
Wood is offline   Reply With Quote
Old 27-12-2018, 13:34   #21
Moderator and Certifiable Refitter
 
Wotname's Avatar

Join Date: Jan 2008
Location: South of 43 S, Australia
Boat: C.L.O.D.
Posts: 20,447
Re: Stray- Current Corrosion, or Galvanic Corrosion, or?????...Help

A reminder the OP initially posted about 15 months ago, let's hope he has resolved the issue by now .
__________________
All men dream: but not equally. Those who dream by night in the dusty recesses of their minds wake in the day to find it was vanity: but the dreamers of the day are dangereous men, for they may act their dreams with open eyes, to make it possible. T.E. Lawrence
Wotname is online now   Reply With Quote
Old 27-12-2018, 16:41   #22
Hull Diver
 
fstbttms's Avatar

Cruisers Forum Supporter

Join Date: Oct 2006
Location: Under a boat, in a marina, in the San Francisco Bay
Posts: 5,434
Re: Stray- Current Corrosion, or Galvanic Corrosion, or?????...Help

Quote:
Originally Posted by CharlieJ View Post
Stray current corrosion is generally a DC phenomenon, it is very destructive to the affected underwater component and generally very fast in its manifestation: days and weeks.
This damage took place in a matter of weeks. The cause? Broken insulation on a 12-volt bilge pump wire.



fstbttms is offline   Reply With Quote
Old 27-12-2018, 16:54   #23
Hull Diver
 
fstbttms's Avatar

Cruisers Forum Supporter

Join Date: Oct 2006
Location: Under a boat, in a marina, in the San Francisco Bay
Posts: 5,434
Re: Stray- Current Corrosion, or Galvanic Corrosion, or?????...Help

Quote:
Originally Posted by Corrosion-Eng View Post
Use an insulation tester or my instrument.
Virtually every post you've made in this forum is a blatant advertisement for your service or product. I suggest you familiarize yourself with the forum rules:

Marine Service Providers may not use any section of the forum to discuss their products or services unless answering a direct question and even in this case may not quote prices or post links, images, videos or contact details in support of that response.
fstbttms is offline   Reply With Quote
Old 27-12-2018, 17:02   #24
Registered User

Join Date: May 2009
Location: Massachusetts
Boat: 40' Silverton Aftcabin with twin Crusaders
Posts: 1,791
Re: Stray- Current Corrosion, or Galvanic Corrosion, or?????...Help

Quote:
Originally Posted by Wood View Post
Assuming aluminum anodes on fiberglass hull 1/2 cell should read -1050 mv or so. Over protection would show > -1200mv or thereabouts.



You can check specs for steel hulls / or different anodes on places like boatzincs.com
Weelll, OK but the max voltage for aluminum is -1.1v. But I get the idea. What troubled me was that adding additional anodes is the same as adding batteries in parallel so the terminal voltage does not change but the current capacity obviously would increase. So it makes sense at least to me that an anode's current is not only determined by the resistance of the solution and the voltage between the anode and the metal under test. It is also because the anode will have a maximum current determined by its surface area.

Greater area, greater current so there would be less voltage dropped in the internal resistance of the anode proper.

Conclusion--- I agree with you!
foggysail is offline   Reply With Quote
Old 19-03-2019, 17:20   #25
Registered User

Join Date: Feb 2017
Posts: 37
Re: Stray- Current Corrosion, or Galvanic Corrosion, or?????...Help

SeaBis electrolysis elimination system is a pretty good gadget to have connected all the time to monitor if and when there is stray DC current. Mine works very well and helps when tracking down suspicious DC equipment.

The device has a built-in AC alarm. As I am never connected to AC shore power, it is only an added unused feature. But whenever the solar panels belt out any higher than 13.8 volts DC, that AC alarm light starts flashing intermittently along with the battery negative side of the monitor and sometimes the positive side as well. If I turn off the solar panels or wait til sundown so their output is below 13.8 volts DC, all goes back to normal.

The seller suggested my solar panels are producing too much AC voltage. I am wondering if anyone out there has the same experience.
Warren Drifter is offline   Reply With Quote
Old 19-03-2019, 18:42   #26
Marine Service Provider
 
boatpoker's Avatar

Join Date: Nov 2008
Location: Port Credit, Ontario or Bahamas
Boat: Benford 38 Fantail Cruiser
Posts: 7,117
Re: Stray- Current Corrosion, or Galvanic Corrosion, or?????...Help

Quote:
Originally Posted by Warren Drifter View Post
SeaBis electrolysis elimination system is a pretty good gadget to have connected all the time to monitor if and when there is stray DC current. Mine works very well and helps when tracking down suspicious DC equipment.

The device has a built-in AC alarm. As I am never connected to AC shore power, it is only an added unused feature. But whenever the solar panels belt out any higher than 13.8 volts DC, that AC alarm light starts flashing intermittently along with the battery negative side of the monitor and sometimes the positive side as well. If I turn off the solar panels or wait til sundown so their output is below 13.8 volts DC, all goes back to normal.

The seller suggested my solar panels are producing too much AC voltage. I am wondering if anyone out there has the same experience.
I had never heard of this system so I had to look it up. As a Certified Marine Corrosion Analyst I have never seen so much snake oil, absolute BS and complete misuderstanding of stray current and electrolytic corrosion in one place. My dock neighbour & buddy (retired two years ago as president of IEEE) just had a look at it together and had a good laugh.

It would literally take me all night to go through the BS on that site one point at a time. Let me just suggest you hire a real Certified Marine Corrosion Analyst before falling for that nonsense.

One tidbit I will offer ... Anyone who uses the term "electrolysis" in relation to electrolytic or stray current corrosion clearly does not understand what the word means. No marine corrosion professional trained in thses matters would use that word as it is a different process altogether.

I'm sure there are some who will argue this point but this is so stupid I will not be replying.
__________________
If you're not laughing, you're not doin' it right.
boatpoker is offline   Reply With Quote
Old 19-03-2019, 18:45   #27
Registered User
 
senormechanico's Avatar

Join Date: Aug 2003
Boat: Dragonfly 1000 trimaran
Posts: 7,163
Re: Stray- Current Corrosion, or Galvanic Corrosion, or?????...Help

Ya gotta get rid of those AC solar panels.

Get some DC panels !!

>sarcasm<
__________________
The question is not, "Who will let me?"
The question is,"Who is going to stop me?"


Ayn Rand
senormechanico is offline   Reply With Quote
Old 19-03-2019, 18:47   #28
Registered User

Join Date: May 2009
Location: Massachusetts
Boat: 40' Silverton Aftcabin with twin Crusaders
Posts: 1,791
Re: Stray- Current Corrosion, or Galvanic Corrosion, or?????...Help

Quote:
Originally Posted by Warren Drifter View Post
SeaBis electrolysis elimination system is a pretty good gadget to have connected all the time to monitor if and when there is stray DC current. Mine works very well and helps when tracking down suspicious DC equipment.

The device has a built-in AC alarm. As I am never connected to AC shore power, it is only an added unused feature. But whenever the solar panels belt out any higher than 13.8 volts DC, that AC alarm light starts flashing intermittently along with the battery negative side of the monitor and sometimes the positive side as well. If I turn off the solar panels or wait til sundown so their output is below 13.8 volts DC, all goes back to normal.

The seller suggested my solar panels are producing too much AC voltage. I am wondering if anyone out there has the same experience.

Did the seller suggest what the AC voltage frequency might be produced by your DC solar panels
foggysail is offline   Reply With Quote
Old 19-03-2019, 18:57   #29
Marine Service Provider

Join Date: Dec 2018
Location: Adelaide, South Australia
Boat: Beneteau Oceanis 5.1
Posts: 24
Send a message via Skype™ to Corrosion-Eng
Re: Stray- Current Corrosion, or Galvanic Corrosion, or?????...Help

Hi Warren,
I am the designer with 2 degrees in corrosion cause elimination and 45 years commercial experience.

The solar cell is generating excessive AC when at full power. If allowed to do so persistently that AC must damage batteries and electronics. This is typical of solar cells from China, at this time. I suggest you contact the manufacturer via the supplier. Mean while avoid excessive use. Keep use to just enough to supply you adequate power.

Glen Bishop of SeaBis.
Corrosion-Eng is offline   Reply With Quote
Old 19-03-2019, 20:33   #30
Senior Cruiser
 
skipmac's Avatar

Cruisers Forum Supporter

Join Date: Oct 2007
Location: 29° 49.16’ N 82° 25.82’ W
Boat: Pearson 422
Posts: 16,306
Re: Stray- Current Corrosion, or Galvanic Corrosion, or?????...Help

Well it has been 30 years since I got a degree in electrical engineering that focused on IC design and fabrication and only a couple of classes touched on solar cells but from all I know about them it is would be completely impossible to produce AC directly from a solar cell. Maybe fluctuating DC (especially if you could get the sun to strobe) but AC, no way.

Again maybe you could get pulsating DC or maybe even some AC from a poorly made or malfunctioning controller but the cell itself, don't think so.

PS Boatpoker. Very impressed that your neighbor is a former president of IEEE.
__________________
The water is always bluer on the other side of the ocean.
Sometimes it's necessary to state the obvious for the benefit of the oblivious.
Rust is the poor man's Loctite.
skipmac is offline   Reply With Quote
Reply

Tags
corrosion, current


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
Stray Current Detector Ian R Electrical: Batteries, Generators & Solar 12 27-12-2018 19:02
Galvanic corrosion or Stray current? NEW PICS!! Captain Pappy Electrical: Batteries, Generators & Solar 7 12-09-2014 13:37
Stray Current MartinMayer Electrical: Batteries, Generators & Solar 32 10-01-2011 04:48
How to Measure Stray Current in the Water erict Electrical: Batteries, Generators & Solar 11 03-12-2010 11:07
Stray Current Corrosion . . . Boracay Electrical: Batteries, Generators & Solar 29 29-09-2010 06:13

Advertise Here


All times are GMT -7. The time now is 05:49.


Google+
Powered by vBulletin® Version 3.8.8 Beta 1
Copyright ©2000 - 2024, vBulletin Solutions, Inc.
Social Knowledge Networks
Powered by vBulletin® Version 3.8.8 Beta 1
Copyright ©2000 - 2024, vBulletin Solutions, Inc.

ShowCase vBulletin Plugins by Drive Thru Online, Inc.