Re: Lost Pencil Zn in Heat Exchanger
Len is happy, but I've got questions. My engine is the only one I know intimately and it doesn't have any zincs, so I know close to less than nothing. Seems anodic protection would only be needed... |
Forum: Engines and Propulsion Systems 23-07-2012, 21:47 |
Replies: 12
Views: 7,614
Posted By
ShipShape
Re: Lost Pencil Zn in Heat Exchanger
If your zinc is in the raw water part of the system and it is 100% zinc it is probably ok to leave it, but if it has some other metal on it, and it probably does, you should remove it. If it is in... |
Showing results 1 to 2 of 2 |
Powered by vBulletin® Version 3.8.8 Beta 1
Copyright ©2000 - 2024, vBulletin Solutions, Inc. |
Privacy Guaranteed - your email is never shared with anyone, opt out any time.