On our boat the blisters are mostly inside the starboard hull,we found about 20,some of them small and then some others about 3 to 5 ",when you start grinding very lightly you can see water starting to come out,and if you go deeper you get into some delamination,so you have to go deeper untill you find some sound fiberglass.I have seen that on many boats,the job needs to be done right so it won't happen in the future when my boat is not anymore under warranty.I am talking with FP so they can take care of the problem.