Cruisers Forum
 

Go Back   Cruisers & Sailing Forums > Engineering & Systems > Construction, Maintenance & Refit
Cruiser Wiki Click Here to Login
Register Vendors FAQ Community Calendar Today's Posts Log in

Reply
  This discussion is proudly sponsored by:
Please support our sponsors and let them know you heard about their products on Cruisers Forums. Advertise Here
 
Thread Tools Search this Thread Rate Thread Display Modes
Old 16-09-2011, 09:51   #1
Registered User
 
Gooosberry's Avatar

Join Date: Mar 2011
Location: Cape Town, South Africa
Boat: 34' sloop
Posts: 22
Apply Anti-Fouling then Re-Splash - How Quickly ?

Any views on how long I can wait after applying anti-fouling before going back to the water?

I have had some advice that no longer than 48 hours - if that is so (is it) what does the delay cause/do - and is there any way to extend the time?
Gooosberry is offline   Reply With Quote
Old 16-09-2011, 10:25   #2
Registered User
 
Vasco's Avatar

Join Date: Apr 2004
Location: Toronto
Boat: CS36Merlin, "La Belle Aurore"
Posts: 7,557
Re: Apply anti-fouling then back in - how quick?

Depends on the type of anti-fouling paint. Read the instructions.
__________________
Rick I
Toronto in summer, Bahamas in winter.
Vasco is offline   Reply With Quote
Old 16-09-2011, 11:49   #3
Registered User

Join Date: Aug 2009
Location: between the devil and the deep blue sea
Boat: a sailing boat
Posts: 20,437
Re: Apply anti-fouling then back in - how quick?

It is all on the can or else read the spec sheet.

b.
barnakiel is offline   Reply With Quote
Old 16-09-2011, 12:42   #4
Resin Head
 
minaret's Avatar

Cruisers Forum Supporter

Join Date: Aug 2007
Location: Seattle WA
Boat: Nauticat
Posts: 7,205
Images: 52
Re: Apply Anti-Fouling then Re-Splash - How Quickly ?

You want the PDS not the MSDS for this info. Here is the product data sheet for my bottom paint. Max splash time is 60 days for it.

http://www.pettitpaint.com/fileshare...ds/1127706.pdf
minaret is offline   Reply With Quote
Old 18-09-2011, 05:08   #5
Registered User
 
Gooosberry's Avatar

Join Date: Mar 2011
Location: Cape Town, South Africa
Boat: 34' sloop
Posts: 22
Re: Apply Anti-Fouling then Re-Splash - How Quickly ?

the paint in question is marketed as International Paints - Unipro - I have researched as much as I can and read the instructions on the can - and NO NOTE of any timelimit for re-immersion, only notes about going back too quickly!
Gooosberry is offline   Reply With Quote
Old 18-09-2011, 17:56   #6
Registered User
 
senormechanico's Avatar

Join Date: Aug 2003
Boat: Dragonfly 1000 trimaran
Posts: 7,162
Re: Apply Anti-Fouling then Re-Splash - How Quickly ?

I asked a Pettit guy one time about why one had to wait 8 hours or whatever.
He said the paint would cure underwater just fine, but the wait time was so the travelift straps wouldn't harm it.
__________________
The question is not, "Who will let me?"
The question is,"Who is going to stop me?"


Ayn Rand
senormechanico is online now   Reply With Quote
Old 18-09-2011, 18:05   #7
Registered User
 
osirissail's Avatar

Join Date: Feb 2009
Location: A real life Zombie from FL
Boat: Gulfstar 53 - Osiris
Posts: 5,416
Images: 2
Re: Apply Anti-Fouling then Re-Splash - How Quickly ?

Your answer is contained in the product sheet:http://www.boatpaint.co.uk/datasheet...Uni-Pro_GB.pdf

DRYING/OVERCOATING INFORMATION
Drying
- - - - - - - - - - - 5ºC - - - 15ºC - - - - 23ºC - - - 35ºC
Touch Dry [ISO] 1hrs - - -45mins - - -30mins - -20mins
Immersion - - - - 7hrs - - - -5hrs - - - 2hrs - - - -2hrs
Note:Max. Immersion Times are as follows: 5-15°C - 3 mths; 23°C - 2 mths; 35°C - 1 mth

- - - - - - - - -
Normally "Max. Immersion Time" means how long you can wait after painting before the paint starts to oxidize and lose effectiveness. So you have "window" between the "Immersion" and "Max Immersion" to work with depending upon the ambient temperature.
osirissail is offline   Reply With Quote
Old 19-09-2011, 04:00   #8
Senior Cruiser
 
GordMay's Avatar

Cruisers Forum Supporter

Join Date: Mar 2003
Location: Thunder Bay, Ontario - 48-29N x 89-20W
Boat: (Cruiser Living On Dirt)
Posts: 49,439
Images: 241
Re: Apply Anti-Fouling then Re-Splash - How Quickly ?

Uni-Pro Antifouling will be touch dry in between 20 minutes to an hour, and may be immersed (boat launched) within 2 Hours (@ 35ºC) to 7 Hours (@
5ºC).
Maximum delay to immersion varies between 1 - 3 Months, depending upon temperature.

See ➥ http://www.boatpaint.co.uk/datasheet...Uni-Pro_GB.pdf
__________________
Gord May
"If you didn't have the time or money to do it right in the first place, when will you get the time/$ to fix it?"



GordMay is online now   Reply With Quote
Old 19-09-2011, 04:55   #9
CLOD
 
sailorboy1's Avatar

Join Date: Jul 2007
Location: being planted in Jacksonville Fl
Boat: none
Posts: 20,419
Re: Apply Anti-Fouling then Re-Splash - How Quickly ?

I was going to look at multi-season paint this year and put it on when the boat gave out of the water in Nov thinking a multi-season wuld be OK to lanuch in the spring.

But sounds like a no go from this thread.
__________________
Don't ask a bunch of unknown forum people if it is OK to do something on YOUR boat. It is your boat, do what you want!
sailorboy1 is offline   Reply With Quote
Old 19-09-2011, 05:24   #10
Registered User
 
osirissail's Avatar

Join Date: Feb 2009
Location: A real life Zombie from FL
Boat: Gulfstar 53 - Osiris
Posts: 5,416
Images: 2
Re: Apply Anti-Fouling then Re-Splash - How Quickly ?

Quote:
Originally Posted by Don Lucas View Post
I was going to look at multi-season paint this year and put it on when the boat gave out of the water in Nov thinking a multi-season wuld be OK to lanuch in the spring.

But sounds like a no go from this thread.
It is really just a function of the particular paint you choose for multi-season. Some hard paints can remain out of the water for extended times while others cannot. Same with "ablative" paints.
- - Even with a hard paint such as Petit Trinidad which oxidizes when left out of water too long, you can get multi-season use with winter time hauled out storage. What you need to do is before re-launching the boat, you use a "scotch-brite" pad to thorough rub the bottom paint to remove the surface oxidized layer and expose a fresh active layer underneath.
osirissail is offline   Reply With Quote
Old 20-11-2011, 09:31   #11
Registered User
 
JamuJoe's Avatar

Join Date: Feb 2008
Location: Durango, CO
Boat: Leopard 42 - JAMU
Posts: 196
Images: 13
Re: Apply Anti-Fouling then Re-Splash - How Quickly ?

I like the "scotch-brite" pad suggestion. My bottom with two coats of Petit Trinidad over primer was only in the water for three months when we hauled out and left her on the hard in Mexico for 18 months. (Not the plan - my extended absence due to medical issues). Now the bottom paint is heavily oxidized & eroded by sun and rain. I'm loath to let the shipyard where she is stored have at her with sanding discs. I wonder if a good scrub with "scotch-brite" pads would be safer and leave me with good adhesion for fresh Petit Trididad? Any experience or suggestions on this approach?
__________________
Safe Sailing,
JamuJoe - Durango, CO
S/V JAMU - Western Caribbean
JamuJoe is offline   Reply With Quote
Old 20-11-2011, 11:18   #12
Registered User
 
osirissail's Avatar

Join Date: Feb 2009
Location: A real life Zombie from FL
Boat: Gulfstar 53 - Osiris
Posts: 5,416
Images: 2
Re: Apply Anti-Fouling then Re-Splash - How Quickly ?

Quote:
Originally Posted by JamuJoe View Post
I like the "scotch-brite" pad suggestion. My bottom with two coats of Petit Trinidad over primer was only in the water for three months when we hauled out and left her on the hard in Mexico for 18 months. (Not the plan - my extended absence due to medical issues). Now the bottom paint is heavily oxidized & eroded by sun and rain. I'm loath to let the shipyard where she is stored have at her with sanding discs. I wonder if a good scrub with "scotch-brite" pads would be safer and leave me with good adhesion for fresh Petit Trididad? Any experience or suggestions on this approach?
Either way works - with a "scotch-brite" pad you can scuff off the oxidized layer and then put a new layer of Trinidad SR on the bottom. I recommend the "SR" version for its slime resistance chemical.
- - With a random orbital sander and 120grit paper you can do the same scuffing quicker than by hand. But like any machine, if it is not operated with care it can dig in and remove a lot more than just the oxidized surface layer.
osirissail is offline   Reply With Quote
Old 21-11-2011, 05:10   #13
Senior Cruiser
 
GordMay's Avatar

Cruisers Forum Supporter

Join Date: Mar 2003
Location: Thunder Bay, Ontario - 48-29N x 89-20W
Boat: (Cruiser Living On Dirt)
Posts: 49,439
Images: 241
Re: Apply Anti-Fouling then Re-Splash - How Quickly ?

See the Petit Instructions
http://www.pettitpaint.com/fileshare...ds/1167706.pdf
__________________
Gord May
"If you didn't have the time or money to do it right in the first place, when will you get the time/$ to fix it?"



GordMay is online now   Reply With Quote
Old 21-11-2011, 05:20   #14
CLOD
 
sailorboy1's Avatar

Join Date: Jul 2007
Location: being planted in Jacksonville Fl
Boat: none
Posts: 20,419
Re: Apply Anti-Fouling then Re-Splash - How Quickly ?

Quote:
Originally Posted by GordMay View Post
Nothing in those directions says the boat can be out of the water more than 60 days and that it's OK to just Scott-Brite the surface if so.
__________________
Don't ask a bunch of unknown forum people if it is OK to do something on YOUR boat. It is your boat, do what you want!
sailorboy1 is offline   Reply With Quote
Old 21-11-2011, 05:30   #15
Senior Cruiser
 
GordMay's Avatar

Cruisers Forum Supporter

Join Date: Mar 2003
Location: Thunder Bay, Ontario - 48-29N x 89-20W
Boat: (Cruiser Living On Dirt)
Posts: 49,439
Images: 241
Re: Apply Anti-Fouling then Re-Splash - How Quickly ?

APPLICATION TEMP: 40° F. Min. / 90°F. Max.
DRY TIME* (HOURS):
Temp. ~ To Recoat ~ To Launch
90°F ~ 2Hrs ~ 8Hrs
70°F ~ 4 ~ 16
40°F ~ 6 ~ 24
*The above dry times are minimums.
Trinidad SR Antifouling may be recoated after the minimum time shown and launched up to 60 days after painting.

Previously Painted Surfaces:
If the previous coating is in good condition, thoroughly sand with 80 grit paper then solvent clean with 120 Brushing Thinner to remove residue. Apply two finish coats of Trinidad SR.
If the previous coating is soft or in poor condition, remove to the bare surface by sanding or using Pettit 9051 Bio Blast Paint Remover. Proceed with appropriate bare system as described below. Old tin copolymers should be removed or sealed with Pettit 6627 Tie Coat Primer before applying Trinidad SR Antifouling.
__________________
Gord May
"If you didn't have the time or money to do it right in the first place, when will you get the time/$ to fix it?"



GordMay is online now   Reply With Quote
Reply

Tags
anti-fouling


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Advertise Here


All times are GMT -7. The time now is 10:38.


Google+
Powered by vBulletin® Version 3.8.8 Beta 1
Copyright ©2000 - 2024, vBulletin Solutions, Inc.
Social Knowledge Networks
Powered by vBulletin® Version 3.8.8 Beta 1
Copyright ©2000 - 2024, vBulletin Solutions, Inc.

ShowCase vBulletin Plugins by Drive Thru Online, Inc.